8years
Full-line delivery experience
11lines
Lines installed
>97%% uptime
Average yield
±10μm
Coating thickness tolerance
Process
Five steps. One compact line.
01
Plasma/Laser cleaning
Atmospheric Ar plasma for de-dusting, de-oiling and surface activation
02
UV coating
Two-component spray coating · tolerance ±10 μm
03
UV curing
405 nm · 800 mJ/cm² dose
04
Inline thickness inspection
3D vision + non-contact thickness testing, 100%
05
Inline HV inspection
High-voltage insulation test, 100%
Cell Coating Pilot Line · Shenzhen
Cell Coating Line
Full-line UV coating
Cycle time>50PPM
Coating thickness120μm
Coating tolerance±10μm
UV wavelength405nm